V weave material


Author
Message
aidanh
a
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 2, Visits: 36
I have a task ahead of me to carbon skin the front end of a car. I need to use v weave on the bonnet and bumper for the project but the bumper is going to need material wider than 1500mm/59''. EC only do it to 1500mm wide and to whatever length you require. Can anyone recommend any other companies that can supply v weave fabric wide enough for this project of mine? The material will need to be roughly 2300mm to fit the bumper. 
scottracing
scottracing
Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
aidanh - 9/16/2020 5:46:26 PM
I have a task ahead of me to carbon skin the front end of a car. I need to use v weave on the bonnet and bumper for the project but the bumper is going to need material wider than 1500mm/59''. EC only do it to 1500mm wide and to whatever length you require. Can anyone recommend any other companies that can supply v weave fabric wide enough for this project of mine? The material will need to be roughly 2300mm to fit the bumper. 

Just use normal 2x2 twill and with decent shears and a bit of spraytack down the cut line. Then do a very smalloverlap or butt joint.
As you are skinning it you should be able to pre wet the material and get it to stay where you need it?

Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeh nobody is going to do 2.5m wide v-weave by the metre, you would have to special order that and buy it in BULK. Easier to just buy regular twill and do as Scott suggests.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search