By aidanh - 9/16/2020 5:46:26 PM
I have a task ahead of me to carbon skin the front end of a car. I need to use v weave on the bonnet and bumper for the project but the bumper is going to need material wider than 1500mm/59''. EC only do it to 1500mm wide and to whatever length you require. Can anyone recommend any other companies that can supply v weave fabric wide enough for this project of mine? The material will need to be roughly 2300mm to fit the bumper.
|
By Hanaldo - 9/16/2020 11:04:24 PM
Yeh nobody is going to do 2.5m wide v-weave by the metre, you would have to special order that and buy it in BULK. Easier to just buy regular twill and do as Scott suggests.
|
|