DD-Compound - 9/12/2020 5:52:09 AM
For the core you can bond 2x10mm together but take care it’s bonded proper, otherwise it will delaminate at neutral axis and you will loose stiffness and make sure the holes are not closed, otherwise your infusion will fail. 

Hi, can you recommend best way to bond PVC foam sheets?
Would micro fibers thickened epoxy do?

(About holes: I will perforate after the bonding, so no problem about closed holes)

Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Massimiliano - 9/14/2020 12:59:31 PM
DD-Compound - 9/12/2020 5:52:09 AM
For the core you can bond 2x10mm together but take care it’s bonded proper, otherwise it will delaminate at neutral axis and you will loose stiffness and make sure the holes are not closed, otherwise your infusion will fail. 

Hi, can you recommend best way to bond PVC foam sheets?
Would micro fibers thickened epoxy do?

(About holes: I will perforate after the bonding, so no problem about closed holes)

Thickened epoxy is fine. It is critical to completely cover both surfaces so you have no voids. And then you need to press the sheets together with a very even pressure - vacuum is the easiest way to achieve this. 

Massimiliano
M
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hanaldo - 9/14/2020 2:16:37 PM
Massimiliano - 9/14/2020 12:59:31 PM
DD-Compound - 9/12/2020 5:52:09 AM
For the core you can bond 2x10mm together but take care it’s bonded proper, otherwise it will delaminate at neutral axis and you will loose stiffness and make sure the holes are not closed, otherwise your infusion will fail. 

Hi, can you recommend best way to bond PVC foam sheets?
Would micro fibers thickened epoxy do?

(About holes: I will perforate after the bonding, so no problem about closed holes)

Thickened epoxy is fine. It is critical to completely cover both surfaces so you have no voids. And then you need to press the sheets together with a very even pressure - vacuum is the easiest way to achieve this. 

Thank you, will do as you suggest!


DD-Compound
DD-Compound
Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)Supreme Being (338 reputation)
Group: Forum Members
Posts: 25, Visits: 1.1K
I would not recommend to bond but if you can also do that during infusion. Place a flow layer between the cores and the resin will bond it during infusion.
Otherwise I would use something like a thixotrop paste, made from aerosil and microballoons with resin.
We sometimes use Gflow500 from Chomarat between the cores of we have to.

http://www.talkcomposites.com/Uploads/Images/f1d078f0-feab-4db2-8f2f-f009.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search