Hello, 
I have one question, please. Is there any danger in terms of deformation of a cured prepreg part, if I will do demoulding before the part and mould reach the room temperature? I mean, for example, if I pull the part out of the mould while the mould temperature is still approx. 100°C (curing at 120°C). For more info, I use prepreg carbon from EasyComposites and use a aluminium mould. Thank you for your help!
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
I release 100C hot pre preg parts all the time with no issue.