By joei.pavlas - 7/29/2020 5:19:44 PM
Hello, I have one question, please. Is there any danger in terms of deformation of a cured prepreg part, if I will do demoulding before the part and mould reach the room temperature? I mean, for example, if I pull the part out of the mould while the mould temperature is still approx. 100°C (curing at 120°C). For more info, I use prepreg carbon from EasyComposites and use a aluminium mould. Thank you for your help!
|
By Fasta - 9/6/2020 1:44:55 AM
I release 100C hot pre preg parts all the time with no issue.
|
|