Peel ply on pre preg


Author
Message
carbon man
carbon man
Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Will this work? Mabe release film then peel ply?

I'm trying to achieve a uniform flat finish on the back on the pre preg part, and not lines of resin that need sanding out to allow the cover to fit. 

I tried release film and then breather and it worked great, but it left the face of the carbon with pin holes in.

Using xpreg xc110.

Thanks


Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It will work in direct contact with the pre-preg if you have enough resin, ie. more than 3 layers of XC110, or use the film adhesive. 
carbon man
carbon man
Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Hanaldo - 7/16/2020 1:23:36 AM
It will work in direct contact with the pre-preg if you have enough resin, ie. more than 3 layers of XC110, or use the film adhesive. 

Thanks, it will only be 1 x surface ply and 1 x backing ply. What is film adhesive? 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon man - 5 Years Ago
Hanaldo - 5 Years Ago
carbon man - 5 Years Ago
Hanaldo - 5 Years Ago
carbon man - 5 Years Ago
Warren (Staff) - 5 Years Ago
explorecomposites - 5 Years Ago
carbon man - 5 Years Ago
explorecomposites - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search