Successfuly made some pre preg. Wanting to clear coat. Untill I get set up I'm using rattle can acrylic.

I key in with 800 grit but it drys showing all the 800 scratches .

Would this still happen with proper mixed 2k clear coat?

Thanks
Replies
beliblisk
b
Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K
carbon man - 7/4/2020 4:36:03 PM
Hanaldo - 7/4/2020 3:12:47 PM
Depends if you use a high solids clear or a medium solids clear. For medium solids you want to prep with a gold scuffing pad rather than sand paper. For high solids, you can prep with 600 grit.

What's the difference? Mainly spraying small parts of that makes a difference 

Like name suggests there is higher solids (HS) content. It is also called scratch resistant clear... i use ultra high solids (UHS) clear to coat CF and can even get away with 400 grit but most of the time i finish at 800. All offcourse 2k.

Edited 5 Years Ago by beliblisk
carbon man
carbon man
Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)Supreme Being (756 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
beliblisk - 7/4/2020 5:42:59 PM
carbon man - 7/4/2020 4:36:03 PM
Hanaldo - 7/4/2020 3:12:47 PM
Depends if you use a high solids clear or a medium solids clear. For medium solids you want to prep with a gold scuffing pad rather than sand paper. For high solids, you can prep with 600 grit.

What's the difference? Mainly spraying small parts of that makes a difference 

Like name suggests there is higher solids (HS) content. It is also called scratch resistant clear... i use ultra high solids (UHS) clear to coat CF and can even get away with 400 grit but most of the time i finish at 800. All offcourse 2k.

Nice thanks. Can you also point me in the right direction for compressor and spray gun. Also what brand of clear coat do you use. Is it acrylic 2k?

beliblisk
b
Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)Supreme Being (563 reputation)
Group: Forum Members
Posts: 53, Visits: 2.8K
Its PU UHS clear....... its our local manufacturer but i am sure you can get it near you in specialized store for car paints & bodyshop equipment. 

Ask for advice on spray gun and compressor there as well. I dont know exactly wgat brand of gun i am using (one small and one big) but can make pics if needed on mondaySmile


Edited 5 Years Ago by beliblisk
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon man - 5 Years Ago
Hanaldo - 5 Years Ago
carbon man - 5 Years Ago
beliblisk - 5 Years Ago
carbon man - 5 Years Ago
beliblisk - 5 Years Ago
Hanaldo - 5 Years Ago
LibertyMKiii - 5 Years Ago
carbon man - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search