Talk Composites - The Forum for Advanced Composites

Clear coat advice.

http://www.talkcomposites.com/Topic37358.aspx

By carbon man - 7/4/2020 3:05:19 PM

Successfuly made some pre preg. Wanting to clear coat. Untill I get set up I'm using rattle can acrylic.

I key in with 800 grit but it drys showing all the 800 scratches .

Would this still happen with proper mixed 2k clear coat?

Thanks
By carbon man - 7/22/2020 8:20:27 PM

LibertyMKiii - 7/17/2020 5:22:54 PM
This one was wet sanded with 600 grit then 2k clear was applied.


Nice! I take that's dried and polished. Air a standard face ok to use. Or do you use air feed?