Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Easylease is a one part system, it's sealer is 'built in' to the release agent so it doesn't need a seperate sealer initially.
In all honesty, there are so many possibilities for what could have caused this that without knowing exactly how the mould was made and everything that went on; we are all just speculating and you won't get an actual answer. For me, it looks like the mould wasn't fully cured. It is what I would expect to see if you tried to make a pre-preg part in a mould that hadn't been post cured first. There's a few things that could have caused that to be the case. Or I could be wrong, and it could be something else.
|