By carbon man - 6/28/2020 7:16:54 AM
Hi, this mould is made from high temp epoxy and oven for 17 hours following the data sheet.
I think I could of took more care in mould prep which didn't help. But it had about 8 coats of easy lease and struggled to out. Now the mould has carbon print through and cracked gel?
Carbon use xpreg xc110 oven cured following standard curing cycle.
Edit : carbon was in the mould over night before going in the oven as it was getting late and could fix leak in the bag.
|
By carbon man - 7/3/2020 7:49:04 PM
Hoping iv solved it! Been using easy lease that's 2 years old.. Didn't even know it expired. So tried again tonight with a new bottle..
|
|