Has anyone experience using XCR Epoxy instead of clearcoat? Is the result comparable?

I have bought „special“ clear coat and filler for epoxy and now I am wondering which is best practice.

Thanks for your opinions!
Replies
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
XCR, being a resin, is a much thicker layer.  Properly sanded smooth XCR with a high quality polish will look very good but generally does not look as "wet" as a clear coat lacquer. 

Also Modern automotive lacquers will generally offer much better UV protection as most are 100% UV stable. Depending on your climate, this may or may not be a consideration.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
SHaas
S
Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)Supreme Being (607 reputation)
Group: Forum Members
Posts: 46, Visits: 384
Warren (Staff) - 4/14/2020 4:33:29 PM
XCR, being a resin, is a much thicker layer.  Properly sanded smooth XCR with a high quality polish will look very good but generally does not look as "wet" as a clear coat lacquer. 

Also Modern automotive lacquers will generally offer much better UV protection as most are 100% UV stable. Depending on your climate, this may or may not be a consideration.

Ok thanks I will try both options and compare the result