Group: Forum Members
Posts: 107,
Visits: 504
|
i did speak to the guy who makes them, he said at first they did use pre-preg to do the engine cover lid but it worked out to expensive (not much profit basically), but the parts that were supplied are done with resin infusion, then autoclaved at 60deg then up to 100deg.
i have pulled some bits plastic sheet that was left in the tight corners
think i might give it a try as i'm ready to do another panel
|