By neilb - 11/26/2012 8:24:55 AM				
            
                      
            we had a gallardo come in at work a few days ago for an updated front bumper and some superleggera mods. basically the superleggera front bumper does'nt fit the older gallardo's so a few company's have done there own, we had one delivered. its a fibreglass bumper with a carbon lower half. its made using infusion but from what i can see its not made with the infusion mesh. it looks like it had a layer of breather fabric on top of the fabric stack then the bagging film.
  is this a short cut?
  i'll post up some pics shortly! 
 
  
 
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By neilb - 12/1/2012 4:51:47 AM				
            
                      
            more pics,
 
  
 
  
 
  
 
  
           
		 | 			
		 
	
	
						
		 	
		
	 |