What is the best technique to mold these parts, and redo them in carbon?
infusion? Prepreg?
Dimensions: 700mm x 350mm
Thank's a lot.

Replies
polaraligned
polaraligned
Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)Supreme Being (112 reputation)
Group: Forum Members
Posts: 13, Visits: 284
If you want a strong door, I would make in one piece with plenty of fiber overlap where direction changes.  I would also used a balanced and symmetric layup.  The 3D core will not make those tight bends, and if you force it, you will have paths for race tracking of the epoxy if you do an infusion.   

Thecydart
T
Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)
Group: Forum Members
Posts: 14, Visits: 155
Thank you, in one piece it is not possible? several layers yes, symmetrical yes, but how many? and what type?
MarkMK
MarkMK
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
The 210g surface layer backed up with a 650g fabric will deliver a part with just under 1mm thickness and on something with narrow widths and angles like that it would feel quite sturdy.

Add in an additional layer of 300g fabric between those plies and it should feel very strong. If you want to be more certain, you can always add in small additional sections of the 300g fabric where you intend to attach anything. The 650g fabric will feel a little less compliant, so be certain to consolidate it well into the corners using a rounded tool of some description






Thecydart
T
Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)Supreme Being (141 reputation)
Group: Forum Members
Posts: 14, Visits: 155
thank you for all this precious information, I'm going to start from the top ;-) Besides, having no weight problem, can I put glass fabrics inside instead of carbon?
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Thecydart - 5 Years Ago
Buchado - 5 Years Ago
Thecydart - 5 Years Ago
Buchado - 5 Years Ago
Hanaldo - 5 Years Ago
                         What about ooa prepreg?
Buchado - 5 Years Ago
Hanaldo - 5 Years Ago
                                 I don't even know what it is ooa !!! 🧐
Thecydart - 5 Years Ago
                                     Out of autoclave prepreg.
Buchado - 5 Years Ago
Thecydart - 5 Years Ago
Thecydart - 5 Years Ago
MarkMK - 5 Years Ago
Thecydart - 5 Years Ago
Thecydart - 5 Years Ago
Buchado - 5 Years Ago
Thecydart - 5 Years Ago
SleepingAwake - 5 Years Ago
Thecydart - 5 Years Ago
                     I understand this.
SleepingAwake - 5 Years Ago
                         but with several folds of carbon fabrics? Shouldn't we see through?
Thecydart - 5 Years Ago
                             thw 210gsm fabric is the visible surface i assume?
SleepingAwake - 5 Years Ago
Thecydart - 5 Years Ago
polaraligned - 5 Years Ago
Thecydart - 5 Years Ago
MarkMK - 5 Years Ago
Thecydart - 5 Years Ago
MarkMK - 5 Years Ago
Thecydart - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search