Hi,
there is no way how a vacuum betweeen two plasic sheets can improve anything but process safety.
Just imagine what happens, when there is no inner vacuum but only the outer vacuum between the two bags. You have no pressure applied from atmosphere, no compaction - nothing.

In wind industry we are talking about infusions with tons of materials - a failed infusion would we very expensive.

BR
Bernd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Classicarbon - 5 Years Ago
hojo - 5 Years Ago
Hanaldo - 5 Years Ago
berndhac - 5 Years Ago
hojo - 5 Years Ago
explorecomposites - 5 Years Ago
berndhac - 5 Years Ago
DD-Compound - 5 Years Ago
             Hey Dominik!, Good to see you here!
hojo - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search