posted 6 Years Ago
ANSWER
HOT
Topic Details
C
Group: Forum Members
Posts: 86,
Visits: 639
https://www.compositesworld.com/articles/double-bag-infusion-70-fiber-volume
Edited
6 Years Ago by
Classicarbon
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Duble bag infiusion process
Classicarbon
-
6 Years Ago
Classic article, but too many people misunderstanding the physics of double vacuum bagging and the main purpose. Unfortunately you cannot have the inner bag at a reduced vacuum level, and have the...
hojo
-
6 Years Ago
Exactly ^ I'm yet to believe this is anything more than 'snake oil'. Totally understand it increases vacuum integrity, and so I can see why companies like Boeing use it because as Hojo said it...
Hanaldo
-
6 Years Ago
Hi, in Wind Industry rotorblade production this is quite common as well. BR Bernd
berndhac
-
6 Years Ago
Yes, as well as making large tools such for wind blade tooling (I was previously R&D/Process manager for Gurit Tooling). Double bagging is important to lower the risk of a failed infusion. The cost t...
hojo
-
6 Years Ago
There's got to be something there besides just safety and redundancy - but I'm not sure what it is. It keeps coming back around too much for something completely bogus! I know it is possible to push....
explorecomposites
-
6 Years Ago
Hi, there is no way how a vacuum betweeen two plasic sheets can improve anything but process safety. Just imagine what happens, when there is no inner vacuum but only the outer vacuum between the two...
berndhac
-
6 Years Ago
First, Hi Howard! Second, there is a very informative thread in another composite forum. Double bag is only for process stability and nothing more. The reason for double bagging is to creat during an...
DD-Compound
-
6 Years Ago
Hey Dominik!, Good to see you here!
hojo
-
6 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search