Yes you can pour subsequent layers when the first layer has reached the B stage. At that point, the heat generated on the first layer should be dissipated enough to not have a significant effect on the second layer.
For ease of use, we would recommend trying to catch the B stage as less preparation is needed and you are less likely to see any line deviation between the layers.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|