Hi,

What is the best way to mark cut lines on pre-preg carbon fibre, to avoid making cuts on the mould.

Some guys at my place use white China markers but I find they aren't very precise, due to being fairly blunt.

Cheers
Steve
MarkMK
MarkMK
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 338, Visits: 2K
I often use a dry-wipe marker pen with a fairly sharp tip. The advantage is that it any traces of the marker can then be polished-off easily. A permanent ink marker, like a 'Sharpie' pen, can be a little harder to clean away

If more precision is required, then you could use something like a scribe or compass point to scratch the lines in, but this leave little room for error in terms of slipping and scratching the part surface

When pulling multiple parts from the same mould, I tend to lightly score the gel coat around the edge of part already cut to size and this will leave ready-made cut lines on subsequent parts


Edited 7 Years Ago by MarkMK
Chris Rogers
C
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 120, Visits: 933
Not sure if you mean scribe lines or marks for trimming material...

For scribe lines thin fine-line tape or one edge of that adhesive teflon (Tooltec) or thin flashbreaker tape is nice for leaving a hard edge to trim to in the finished part.  The teflon (with yellow backer) is nice because it peels off more easily than most things after a cook.

I have used thin (1-2mm) sheets of HDPE or similar hard plastic to trim prepreg ply edges and laps in the mold.  You mark the cut with a slip sheet of backer in there and then peel back, lay the (pretty bendy) piece of plastic right in to cut against.  Works best with woven but ok with uni if you leave your backer on.  




f1rob
f1rob
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Most materials you can get a black or blue biro to show up fairly well
If you want to go the "crayon" route use verethin 
They are solid pigment not wax based like chinagraph. Gold (no99 I belive) shows up well,you can sharpen them like a normal pencil
YouStoleMyMash
Y
Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)Supreme Being (99 reputation)
Group: Forum Members
Posts: 8, Visits: 195
f1rob - 11/26/2019 9:36:08 PM
Most materials you can get a black or blue biro to show up fairly well
If you want to go the "crayon" route use verethin 
They are solid pigment not wax based like chinagraph. Gold (no99 I belive) shows up well,you can sharpen them like a normal pencil

Just got some Verithin pencils and they're working pretty well. Thanks