By YouStoleMyMash - 11/24/2019 10:38:15 PM

Hi,

What is the best way to mark cut lines on pre-preg carbon fibre, to avoid making cuts on the mould.

Some guys at my place use white China markers but I find they aren't very precise, due to being fairly blunt.

Cheers
Steve
By YouStoleMyMash - 12/9/2019 9:11:07 AM

f1rob - 11/26/2019 9:36:08 PM
Most materials you can get a black or blue biro to show up fairly well
If you want to go the "crayon" route use verethin 
They are solid pigment not wax based like chinagraph. Gold (no99 I belive) shows up well,you can sharpen them like a normal pencil

Just got some Verithin pencils and they're working pretty well. Thanks