Trying to figure out how to keep the bag to stay tight all the way through the infusion process. there’s absolutely no leaks before we start infusing the resin. But as soon as we open up the resin inlet line the inlet side/area of the bag loosens up and it really never get a tight until the resin starts to gel. Anyone have this issue or does anyone know how to fix this issue. I’m finding small pitting on the surface and only on the inlet side so i’m guessing g it’s happening from the bag being loose on that side.
Reply
mscomposites
m
Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)Supreme Being (169 reputation)
Group: Forum Members
Posts: 23, Visits: 108
Yah I like the fact of keeping vacuum on without drawing out any resin. Will see what we get on these next couple of parts going to try locking off vacuum and allowing more resin to flow in before locking off the resin inlet.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mscomposites - 5 Years Ago
Hanaldo - 5 Years Ago
mscomposites - 5 Years Ago
mscomposites - 5 Years Ago
SleepingAwake - 5 Years Ago
mscomposites - 5 Years Ago
MarkMK - 5 Years Ago
mscomposites - 5 Years Ago
SleepingAwake - 5 Years Ago
MarkMK - 5 Years Ago
FrankZane - 5 Years Ago
MarkMK - 5 Years Ago
mscomposites - 5 Years Ago
Hanaldo - 5 Years Ago
mscomposites - 5 Years Ago
mscomposites - 5 Years Ago
Hanaldo - 5 Years Ago
mscomposites - 5 Years Ago
Hanaldo - 5 Years Ago
mscomposites - 5 Years Ago
SleepingAwake - 5 Years Ago
mscomposites - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search