Hello, I have been working many years with the unimould system but now I going over to the High Temp mould system for the xpreg prepregs .
I am laminating the mould with 1 layer 100G woven glass than 1 layer 280G woven glass after this I let it set to gell han I put 2 layers of 400G woven glass and stop with 1 layer 100G glass to finish.
Are this enough layers for the moulds ? And also "why I dont like epoxy " is there a way to not get the air coming up to the high spots in the moulds . I make superbike fairings and they got alot of shard , round edges and when the glass and epoxy is just layed down , I dont got any airbubbles but after time the wil show up at high spots .
This is why I first put the 100G and 280G and leave them to gell first .
|