Group: Forum Members
Posts: 1,
Visits: 101
|
Hi,
Is it possible to cure prepregs that are supposed to be used in an autoclave using an oven? The manufacturer recommends 85 psi of autoclave pressure and 177 degrees C temperatures for curing and I'm wondering how critical the pressure is to achieve good results.
|