			            This is a very interesting topic. I have some questions regarding this: 1) as to the mentioned biobased epoxies, are they biobased backbone structured epoxies or just using biobased toughener?  biobased epoxies 2) what is the life span for these vehicles? they are niche vehicles and deemed not to be scrapped, but realistically 30 years max 3) have you tried biobased VEs, are they more promising in this application compared to biobased epoxies? no not yet, but i will speak to our team here!                
			            				
			                                 
                     
                                            
                         
                    
                  
             |