This is a very interesting topic. I have some questions regarding this:
1) as to the mentioned biobased epoxies, are they biobased backbone structured epoxies or just using biobased toughener?  biobased epoxies
2) what is the life span for these vehicles? they are niche vehicles and deemed not to be scrapped, but realistically 30 years max
3) have you tried biobased VEs, are they more promising in this application compared to biobased epoxies? no not yet, but i will speak to our team here!
cruxpolymer
c
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 3, Visits: 17
scottracing - 10/1/2019 9:15:05 AM
Im getting a lot more requests at work for suitable bio - sustainable resin systems. Especially the automotive guys, weve used bio based epoxies but we are looking for something more useful for recycling at the end of life of the vehicle.


This is a very interesting topic. I have some questions regarding this:
1) as to the mentioned biobased epoxies, are they biobased backbone structured epoxies or just using biobased toughener?
2) what is the life span for these vehicles?
3) have you tried biobased VEs, are they more promising in this application compared to biobased epoxies?
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
Im getting a lot more requests at work for suitable bio - sustainable resin systems. Especially the automotive guys, weve used bio based epoxies but we are looking for something more useful for recycling at the end of life of the vehicle.

cruxpolymer
c
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 3, Visits: 17
scottracing - 9/30/2019 8:42:47 AM
welcome to the forum, what type of resins are you a specialist in? Epoxy / PU/ Vinylester / BMI ?? 

Hi, Warren and Scottracing, Thanks for reaching out. I have a hands-on experience of Epoxy/VE/BMI. Others include acrylate and cyanate ester. It is nice to meet you guys here and gain deeper understanding of  these resins.

scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
welcome to the forum, what type of resins are you a specialist in? Epoxy / PU/ Vinylester / BMI ?? 

Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Welcome to the forum! Hopefully you will find the answers to your questions here.  We have a large wealth of experience from members and staff so should be able to help with most issues. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
cruxpolymer
c
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 3, Visits: 17
Hi all,

 I am from BC Canada and want to interact with you guys regarding the composite techonologies, and we may also have some cooperations in the future.

Best,
Crossing
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search