Alright Guys, got another question I cant seem to figure out.

I have made a mold for an access cover for the elise. I want to offer this to companies or Race teams with thier logo indented on the part. Also if possible I would like to use the same mould for diffrent layouts so the lettering on the mould would need to be removable.

Here's my thought, theres this machine my hommies girl uses for scrapbooking. It cuts out perfect little letters from pc font.

I want to tsk these little things about 3mm thick and glue them on to make my mold or part.

This is my insperation:

http://www.talkcomposites.com/Uploads/Images/bf97290e-b3d3-4334-be8c-ffdd.jpg

So I want to put in an indent, I have my blank mould made. Now I want to make a part that says "Carbon Tuner" up the side of the part. I would like to take these letters glue them to the mould then make my part from there. I am pretty sure though these little foam letters would compress so I would have to soak them in a hardener of some sort.

In theroy my part would then have the impression, then I could scrape the letters of my mould and be ready for the next logo/name.

And if you wanted it to be rasied well you would have to put the lettering on the donar part before making the mold.

Sorry for lack of a better picture but it cuts out smaller letters like this. Sorry kid, your gonna be famous some day becasue of this:

http://www.talkcomposites.com/Uploads/Images/8e1aea84-4602-494e-b9b4-b58c.JPG



If Brute Force Isn''''t working your not using enough...
Edited 14 Years Ago by Carbon Tuner
Reply
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
I'm a bit worried about sharp edges on letters, and then bridging. Especially with 3mm thick. Why not make a flat plate of carbon fiber and have waterjet the letters, then glue 'em on your part? Maybe the letters made from something like carbon/red poly twill weave to give a little pop?

Just my 2 cents BigGrin

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Carbon Tuner - 14 Years Ago
Joe - 14 Years Ago
Carbon Tuner - 14 Years Ago
Joe - 14 Years Ago
Carbon Tuner - 14 Years Ago
adamsteenfeldt - 14 Years Ago
Bonobo - 14 Years Ago
Carbon Tuner - 14 Years Ago
adamsteenfeldt - 14 Years Ago
jay, - 14 Years Ago
adamsteenfeldt - 14 Years Ago
fgayford - 14 Years Ago
Ragece - 14 Years Ago
jay, - 14 Years Ago
jay, - 14 Years Ago
FLD - 14 Years Ago
fgayford - 14 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search