+x Hanaldo - 7/31/2019 11:49:57 PM240g is the better material in my opinion. Tighter weave, so less fraying and fibre distortion, less gaps between the weave. Easier to handle and has a more 'premium' appearance.Really no difference to the finished part in terms of thickness or strength, the only disadvantage vs the 200g is cost.
+x azcarbonfiber - 7/31/2019 11:51:58 PM+x Hanaldo - 7/31/2019 11:49:57 PM240g is the better material in my opinion. Tighter weave, so less fraying and fibre distortion, less gaps between the weave. Easier to handle and has a more 'premium' appearance.Really no difference to the finished part in terms of thickness or strength, the only disadvantage vs the 200g is cost.That is great news. I appreciate your reply, thank you.