By azcarbonfiber - 7/31/2019 10:31:26 PM

Hello TC!
Can someone please give me some insight to the difference between these two for auto body parts? In the tutorial the parts were made with 200g. Would 240g be too thick and create a problem? Could the 240g also be used? Would there be any disadvantages or advantages in using 240g instead of 200g? Thank you!

Matthew
By MarkMK - 8/3/2019 12:35:55 PM

240g every time and well worth the additional cost if you're aiming for the best possible cosmetics

It looks better and is way more stable to handle and make sharp cuts in