Hi, I want to make my model boat hull using the carbon prepeg and aramid honeycomb sandwich method. I need to fill the honeycomb cells with epoxy in various places were i have penetrators or high stresed load areas so i need to do it in stages. what is the best lay up sequence ? should I lay and cure the outer skin with peel ply then vacuum the honeycomb on after using adhesive film?or a wet lay of epoxy, then cured fill the aramid cells with epoxy were needed. Then apply the prepeg outer skin last without any adhesive.
Or can i lay up the outer skin and honeycomb in one go. would this give the outer skin a good finish. ive looked all over the net for the pre peg honeycomb method but have had no luck, lease advise me the best sequence.
|