Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I have tried Megapoxy HX before. Infused great, but the final composite component was extremely flexible, especially for the first 5 or 6 days. After that, or after a post cure, it was a bit stiffer but still no where near what I would have expected for the layup. I was only doing test panels, but I would be concerned about the potential for distortion.
|