By Mohame - 7/5/2019 1:43:29 PM
Kindly tell me...if very low viscosity epoxy used for injection of cracks in building can be used successfully in vacuum infusion...or any experience of usage ...thanks
|
By Hanaldo - 7/5/2019 11:43:11 PM
I have tried Megapoxy HX before. Infused great, but the final composite component was extremely flexible, especially for the first 5 or 6 days. After that, or after a post cure, it was a bit stiffer but still no where near what I would have expected for the layup. I was only doing test panels, but I would be concerned about the potential for distortion.
|
|