My epoxy is not shiny anymore :(


Author
Message
max Muster
max Muster
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 1, Visits: 12
Good morning, 

After sanding my epoxy resin and I polish it with top finish 2, is my epoxy not anymore shiny. It does not shine any more it is matt now Sad 

Please can help me, someone?
Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
max Muster - 6/27/2019 9:45:55 AM
Good morning, 

After sanding my epoxy resin and I polish it with top finish 2, is my epoxy not anymore shiny. It does not shine any more it is matt now Sad 

Please can help me, someone?

Make sure the resin is fully cured (evt. post curing cycle) as green resin won't take a full gloss, and on top of that the sanding dust is way worse for you...