max Muster
max Muster
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 12
Good morning,
After sanding my epoxy resin and I polish it with top finish 2, is my epoxy not anymore shiny. It does not shine any more it is matt now
Please can help me, someone?
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
My epoxy is not shiny anymore :(
max Muster
-
7 Years Ago
Good morning Max, Thank you for getting in contact. The reason this may have happened could be that when you were sanding the resin, you may have gone up in grits to fast and missing some coarse...
Tom (Staff)
-
7 Years Ago
Make sure the resin is fully cured (evt. post curing cycle) as green resin won't take a full gloss, and on top of that the sanding dust is way worse for you...
SleepingAwake
-
7 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search