In the pictures I can see it just looks like a flat sheet of aluminium with a gurney flap on the rear and end plates riveted on.
Cored material is the way to go. Keeps the weight down.
You could use and off the shelf cored panel if you wanted, but judging from the pictures its only 1 or 2mm aluminium so an off the shelf carbon sheet would do it. Use some angle to create the gurney flap and some offcuts to make the endplates.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|