Foam core with kevlar patches to help reduce rip through of the fixings should be plenty for that kind of application.

The truck might be powerful but I doubt it has massive high speed due to being an aerodynamic brick (compared to a sportscar). As long as it is reasonably stiff and properly mounted to the body then it should stay nicely in place and transfer the downforce to the frame without excessive flex.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
JasonFL
JasonFL
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 51, Visits: 707
Thanks! I was leaning towards a core. Also thinking about strips of Kevlar (sandwiched between the carbon) where the hardware will be attached. His truck has around 750 bhp so I’m going to assume it will see some decent downforce along the way.

Jason
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
In the pictures I can see it just looks like a flat sheet of aluminium with a gurney flap on the rear and end plates riveted on.  

Cored material is the way to go.  Keeps the weight down. 

You could use and off the shelf cored panel if you wanted, but judging from the pictures its only 1 or 2mm aluminium so an off the shelf carbon sheet would do it. Use some angle to create the gurney flap and some offcuts to make the endplates. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
JasonFL
JasonFL
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 51, Visits: 707
A friend of mine wants me to build the wing in this photo for his F100.

Would you make this as a single flat sheet with a cosmetic layer followed by several layers of heavy cloth, or, 2 layers of Carbon, PVC core, and 2 layers of carbon? Hardware is on him to figure out. Just talking the layup.

Deadline is August for a 250 mile rally run up a highway.

Sorry couldn’t get the pic to load but here is the truck:
https://www.hotrod.com/articles/ken-block-hoonitruck/

Jason
Edited 6 Years Ago by JasonFL
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search