Hello,
               I want to infuse and long thin item, circa 1 metre long and 50mm wide. It will have  a Soric core with layers of carbon 2/2 twill either side. Is best to either  feed resin along one edge, along the centre line from one end, from the middle to both ends or something I have not considered yet?

Trevor
Replies
JasonFL
JasonFL
Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)Supreme Being (443 reputation)
Group: Forum Members
Posts: 51, Visits: 707
1 meter resin line on one side, 1 meter vacuum line along the other. Leaves no imprint on the final cloth, and only 50 mm of distance to cover after the resin line is full.

Jason
Trevor Harris
Trevor Harris
Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)Supreme Being (153 reputation)
Group: Forum Members
Posts: 22, Visits: 116
JasonFL - 5/10/2019 8:32:07 PM
1 meter resin line on one side, 1 meter vacuum line along the other. Leaves no imprint on the final cloth, and only 50 mm of distance to cover after the resin line is full.

Hello Jason FL ,
                           Thank you for the info will give it a go.
Trevor