Hello,
               I want to infuse and long thin item, circa 1 metre long and 50mm wide. It will have  a Soric core with layers of carbon 2/2 twill either side. Is best to either  feed resin along one edge, along the centre line from one end, from the middle to both ends or something I have not considered yet?