Mechanical properties of High Strength Carbon Fibre Sheet 2mm 250 x 225mm


Mechanical properties of High Strength Carbon Fibre Sheet 2mm 250 x 225mm
Author
Message
marilyne16
m
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 4, Visits: 19
Hi,

I have some CFRP plates (High Strength Carbon Fibre Sheet 2mm 250 x 225mm) from EasyComposites. I would like to do some finite element modeling simulation, but the properties shared on the easycomposites website are very very limited.

Is it possible to get the accurate mechanical properties of the plate, like the orthotropic elasticity, strain and stress limits, damping factors...?

Thanks and regards,

Marilyne

Replies
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unfortunately we do not have a set of mechanical testing data for these sheets as yet.  We are hoping to do some testing in the coming months which should provide some figures you can use.  

In the mean time, we specify the exact sheet lay up and fabric used on the sheet specification.  Combine that data with the IN2 infusion resin mechanical data and you should be able to calculate some figures to work with until you can do some actual testing.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
marilyne16
m
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 4, Visits: 19
Warren (Staff) - 5/2/2019 9:19:00 AM
Unfortunately we do not have a set of mechanical testing data for these sheets as yet.  We are hoping to do some testing in the coming months which should provide some figures you can use.  

In the mean time, we specify the exact sheet lay up and fabric used on the sheet specification.  Combine that data with the IN2 infusion resin mechanical data and you should be able to calculate some figures to work with until you can do some actual testing.

Thank you. I hope you will be able to provide some data.
Indeed, I tried to calculate the matrix ABBD by lamination theory but I had to implement a lot of assumptions and I would like to correlate with actual results.

Acroflight
A
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 4
marilyne16 - 5/2/2019 9:56:48 AM
Warren (Staff) - 5/2/2019 9:19:00 AM
Unfortunately we do not have a set of mechanical testing data for these sheets as yet.  We are hoping to do some testing in the coming months which should provide some figures you can use.  

In the mean time, we specify the exact sheet lay up and fabric used on the sheet specification.  Combine that data with the IN2 infusion resin mechanical data and you should be able to calculate some figures to work with until you can do some actual testing.

Thank you. I hope you will be able to provide some data.
Indeed, I tried to calculate the matrix ABBD by lamination theory but I had to implement a lot of assumptions and I would like to correlate with actual results.

Hi marilyne16
I am trying to do the same as yourself.  Ideally the XC110 will be able to correlate to similar material in the NIAR database, this will enable me to conduct some stress/FEM work with confidence.  AT this time, without any tests this interesting material is to be either used a) at risk or b) for non-flying parts only.  Option a) will require some heavy knock-downs to the NIAR baseline.

marilyne16
m
Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)Forum Member (45 reputation)
Group: Forum Members
Posts: 4, Visits: 19
Warren (Staff) - 5/2/2019 9:19:00 AM
Unfortunately we do not have a set of mechanical testing data for these sheets as yet.  We are hoping to do some testing in the coming months which should provide some figures you can use.  

In the mean time, we specify the exact sheet lay up and fabric used on the sheet specification.  Combine that data with the IN2 infusion resin mechanical data and you should be able to calculate some figures to work with until you can do some actual testing.

Hi, you are talking about the IN2 infusion resin. Can I know the maximum temperature this resin can be used at once cured in the plate? (i.e. what is the maximum temperature the plate can be heated at?)

Thanks,

Marilyne

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
marilyne16 - 7 Years Ago
oekmont - 7 Years Ago
marilyne16 - 7 Years Ago
Warren (Staff) - 7 Years Ago
marilyne16 - 7 Years Ago
Acroflight - 7 Years Ago
marilyne16 - 7 Years Ago
Warren (Staff) - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search