Hey, Im sculpting this half mask and then making a brush up silicone mould with fiberglass jacket and then using fast cast for casting. Im not sure if its better to mould it as one piece or should I divide it into three sections. Also what silicone is best for brush up mould? Thank you for any help/advices.

Fasta
Fasta
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
UpsettiSpaghetti - 4/21/2019 6:28:36 PM
Hey, Im sculpting this half mask and then making a brush up silicone mould with fiberglass jacket and then using fast cast for casting. Im not sure if its better to mould it as one piece or should I divide it into three sections. Also what silicone is best for brush up mould? Thank you for any help/advices.

You can do the silicone surface mould as one piece and the fibreglass jacket maybe with just two pieces, left and right?

This is one I have done a while ago but it is two piece silicone and jacket.






Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
LIke fasta said, the silicone should be flexible enough to demould that no problem and have a 2 piece solid jacket for ease of use. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search