Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Resin Casting and Moulding Forum
»
General Moulding and Casting Discussion
»
Advice for making a mould + what kind of silicone for brush up
Advice for making a mould + what kind of silicone for brush up
Post Reply
Like
7
Advice for making a mould + what kind of silicone for brush up
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
UpsettiSpaghetti
U
UpsettiSpaghetti
posted 7 Years Ago
ANSWER
HOT
Topic Details
U
Group: Forum Members
Posts: 2,
Visits: 14
Hey, Im sculpting this half mask and then making a brush up silicone mould with fiberglass jacket and then using fast cast for casting. Im not sure if its better to mould it as one piece or should I divide it into three sections. Also what silicone is best for brush up mould? Thank you for any help/advices.
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Advice for making a mould + what kind of silicone for brush up
UpsettiSpaghetti
-
7 Years Ago
You can do the silicone surface mould as one piece and the fibreglass jacket maybe with just two pieces, left and right? This is one I have done a while ago but it is two piece silicone and jacket.
Fasta
-
7 Years Ago
LIke fasta said, the silicone should be flexible enough to demould that no problem and have a 2 piece solid jacket for ease of use.
Warren (Staff)
-
7 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search