Hi all,

Just a quick one.
I infused some small items recently, approx 300mm x 150mm with:
650g 2 twil (mould surface)
3 layers of 200 unidirectional
Then top layer of 450 2
I then added peel ply and infusion mesh.

The top surface just about wetted out, but the mould surface didn’t wet at all.

Is there a particular problem I’m having or is there perhaps a way to slow the resin flow to allow it to saturate all layers?

Many thanks,

Bill

Reply
Lester Populaire
L
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
Rich (Staff) - 4/21/2019 12:01:06 PM
The problem is more likely as a result of your UD layers; assuming they're running in the same direction, the fibres lock together under vacuum making a somewhat impenetrable layer that the resin can't get through which results in dry areas on the mould surface.

While this certainly doesn't help it is certainly possible to infuse near void free. I do this regularly as i like to work with UD layers.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
DorsetBill - 7 Years Ago
SleepingAwake - 7 Years Ago
JasonFL - 7 Years Ago
DorsetBill - 7 Years Ago
JasonFL - 7 Years Ago
DorsetBill - 7 Years Ago
DorsetBill - 7 Years Ago
JasonFL - 7 Years Ago
Rich (Staff) - 7 Years Ago
SleepingAwake - 7 Years Ago
Hanaldo - 7 Years Ago
Fasta - 7 Years Ago
DorsetBill - 7 Years Ago
JasonFL - 7 Years Ago
DorsetBill - 7 Years Ago
JasonFL - 7 Years Ago
DorsetBill - 7 Years Ago
JasonFL - 7 Years Ago
DorsetBill - 7 Years Ago
Fasta - 7 Years Ago
DANNYHOCKIN - 7 Years Ago
DorsetBill - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search