+x CmCarbon - 4/3/2019 9:57:33 AMLooks like you've applyed resin after the tackyness has gone so it hasn't bonded to the previous resin coat.Xcr resin by any chance?
+x CmCarbon - 4/3/2019 10:14:52 AMTry pic of any loose resin and sand it back.. then reapply another few coats of resin
+x Matthieu Libeert - 4/4/2019 7:12:30 AMwhen you wet it out with just a bit of water, do you still see the marks? if not you are ok to apply next layers on top. It is probably where you've sanded through different coats