posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 37,
Visits: 939
hi guys,
was wondering how trim clips are made?
are they part of a two piece mold, or are they made using a separate type of mold (e,g vacuum form or silicone mold) and then stuck onto the carbon fiber part?
Reply
Like
3
Reply
scottracing
scottracing
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
sounds like a lot of hassle, I would 3d print the clips and bond them on.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
how would you make trim clips (see pics)
8900120d
-
6 Years Ago
This is done with injection moulding. complex and expensive moulds with in-mould slides that retract for demoulding, this is used for mass production. Looks like these are carbonfiber pieces with a.....
matthieutje65
-
6 Years Ago
looks like an over moulded part that press forms the skin then with a suitable material moulds the clips on the back, we have the kit at work but the tooling costs are high as matthieu says due to al...
scottracing
-
6 Years Ago
thanks for the replies, isnt there a way to DIY make the clips? i was thinking about using Plasticine to block the holes and make each clip into a "block", then make a vacuum formed plastic mold of.....
8900120d
-
6 Years Ago
sounds like a lot of hassle, I would 3d print the clips and bond them on.
scottracing
-
6 Years Ago
I make silicone moulds with CS25 and then cast them withXencast P6 Toughened Polyurethane Casting Resin. When they are cured i just epoxy them with a bit of carbon fiber wave on to the part
Capitao
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search