Good morning, recently installed a penny floor using Glasscast 3 and couldn’t be happier with the result. Came up with idea of putting map in the entry floor with some postcards and pouring Glasscast 3 over it. Have a few concerns/ questions- there are going to be areas of the underlayment (3/8” AC plywood) that will not be covered by the map/ postcards. My thought was to simply paint entire area either white or black with latex paint to seal wood and then lay down map & postcards. Is it ok to use latex paint for this or should I use something else. Should I glue down the map & cards prior to pouring to eliminate shift or even product getting under items and if so what should I use for adhesive? Thank you in advance for your time, Mike.

Reply
tilegeek
t
Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)Forum Member (27 reputation)
Group: Forum Members
Posts: 4, Visits: 7
Warren (Staff) - 3/12/2019 5:04:58 PM
A good point Okemont has highlighted is colour change of the resin. Many paper grades will soak up resin going semi-translucent or wetting out the colours.  I would recommend testing a small piece to be sure. If it does soak in, coating the paper with a thin layer of PVA wood glue works as a good sealant. In a thin brush on layer, it dries clear.


Thank you for the advice & heads up. I will definitely test the map prior to pouring.