No, anything without a separate hardener component is somehow soluted and will outgas for a long time. You could use the epoxy you already have with black pigments to get a black 2k paint.

tilegeek
t
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 4, Visits: 7
oekmont - 3/12/2019 2:03:03 PM
I would use either black epoxy or polyurethane coating, like it is available for skinning purposes. Latex paint isn't solvent free, wich can end up in bubbles or milky resin.
For the same reason I would use 5 min epoxy to glue them down.
I would check if the postcards are resistant to the epoxy. I had cloths and prints that completely changed colour after epoxy exposure.


Sorry, still working through this- would acrylic paint be a better choice? Thank you again.

tilegeek
t
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 4, Visits: 7
Warren (Staff) - 3/12/2019 5:04:58 PM
A good point Okemont has highlighted is colour change of the resin. Many paper grades will soak up resin going semi-translucent or wetting out the colours.  I would recommend testing a small piece to be sure. If it does soak in, coating the paper with a thin layer of PVA wood glue works as a good sealant. In a thin brush on layer, it dries clear.


Thank you for the advice & heads up. I will definitely test the map prior to pouring.

tilegeek
t
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 4, Visits: 7
oekmont - 3/12/2019 2:03:03 PM
I would use either black epoxy or polyurethane coating, like it is available for skinning purposes. Latex paint isn't solvent free, wich can end up in bubbles or milky resin.
For the same reason I would use 5 min epoxy to glue them down.
I would check if the postcards are resistant to the epoxy. I had cloths and prints that completely changed colour after epoxy exposure.


Thank you for the advice, poly will work instead of paint for the area.


Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A good point Okemont has highlighted is colour change of the resin. Many paper grades will soak up resin going semi-translucent or wetting out the colours.  I would recommend testing a small piece to be sure. If it does soak in, coating the paper with a thin layer of PVA wood glue works as a good sealant. In a thin brush on layer, it dries clear.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
oekmont
oekmont
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
I would use either black epoxy or polyurethane coating, like it is available for skinning purposes. Latex paint isn't solvent free, wich can end up in bubbles or milky resin.
For the same reason I would use 5 min epoxy to glue them down.
I would check if the postcards are resistant to the epoxy. I had cloths and prints that completely changed colour after epoxy exposure.

tilegeek
t
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 4, Visits: 7
Good morning, recently installed a penny floor using Glasscast 3 and couldn’t be happier with the result. Came up with idea of putting map in the entry floor with some postcards and pouring Glasscast 3 over it. Have a few concerns/ questions- there are going to be areas of the underlayment (3/8” AC plywood) that will not be covered by the map/ postcards. My thought was to simply paint entire area either white or black with latex paint to seal wood and then lay down map & postcards. Is it ok to use latex paint for this or should I use something else. Should I glue down the map & cards prior to pouring to eliminate shift or even product getting under items and if so what should I use for adhesive? Thank you in advance for your time, Mike.