A good point Okemont has highlighted is colour change of the resin. Many paper grades will soak up resin going semi-translucent or wetting out the colours. I would recommend testing a small piece to be sure. If it does soak in, coating the paper with a thin layer of PVA wood glue works as a good sealant. In a thin brush on layer, it dries clear.