Hello,
I have a piece made of forged composite (carbon fiber) and it is used in motorsport and I need to make a piece of it using the traditional carbon fiber fabric, this piece has 2mm, I would like to know how many layers of carbon fiber it takes to have a similar mechanical property?
I intend to use carbon fiber with weights 200 g / m² and 300 g / m² and epoxy resin.
The manufacturing process will be done by vacuum infusion using silicone bag membrane because of the large scale manufacturing of that part.
|