Composite Forged versus Carbon Fiber tradicional


Author
Message
Dezer
Dezer
Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)Supreme Being (704 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Hello,

I have a piece made of forged composite (carbon fiber) and it is used in motorsport and I need to make a piece of it using the traditional carbon fiber fabric, this piece has 2mm, I would like to know how many layers of carbon fiber it takes to have a similar mechanical property?

I intend to use carbon fiber with weights 200 g / m² and 300 g / m² and epoxy resin.

The manufacturing process will be done by vacuum infusion using silicone bag membrane because of the large scale manufacturing of that part.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search