I have been trying to cover this in carbon fibre using the Easy Composites XCR Skinning kit and failed on the last two attempts!!... When laying the carbon cloth I have been working from the centre outwards as suggested but I continue to get creases/bridging and all sorts of problems... should I be trying to do this in two or more pieces? or is it my technique?? (or lack of)!! .... where is the best place to start from and what method would you suggest??...
Reply
Peter Robinson
P
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 7, Visits: 65
Warren (Staff) - 2/4/2019 11:07:11 AM
The shape is quite complicated at the front so you might do better using 2 pieces of cloth. One piece for the front detailed area and the second for the smoother rear.


Thanks for your reply... I will give it a try and let you know how I get on!!… If I use two pieces of cloth, would it be better to use a but join or overlap the two pieces where they meet?

Many thanks

Pete
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search