Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Overlapping is generally neater. You can use hairspray or similar on the edge to be cut neatly to help it reduce fraying then carefully overlap that on top the lower fabric and you should have a fairly crisp join line that looks neat.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|