Hi everybody,
I have all the time problems to get a perfect sealed vacuum bag. I think there was only one perfect bag in the last two months...
Now I am thinking about switching to an envelope bag in a pretty big size. I thought of backing the mould with breather to prevent little holes depending on the few sharp pieces on the backside. It also could be that the mould itself is not airtight because I had a crack to repair but I sprayed some layers of board sealer on the whole surface so it should be fine.